3D model description
GOPRINT test model explanation
-
Note: If the column is not straight, there is the following possibilities
1 / screw is not straight, there is a misplaced position
2 / cleaning problem
3 / Insufficient exposure, soft resin, rising deformation -
Measuring the diameter of this row, refer to resin precision
If the size is small, it can be increased
If the size is large, it can be reduced. -
If the vertical face is not circled, then adjust the lift speed.
-
Situation 1: Machine Z screw polarization value is not allowed, or the platform is uneven
Situation 2: Upper speed / lack of exposure, leading to the formation of Kongle -
If there is no appearance of small characters, it is insufficient
-
Measuring film adhesion
-
The parameters of the actual model are preferably blocked by these two holes.
-
This row special test stacked, but if the cleaning is not in place, it will also be bonded
-
This has a row of detail small pits special test resin precision
GoPrint測試模型解說
-
注: 如柱子出現不直情况,有以下可能性
1/絲杆不直,出現錯位
2/ 清洗時碰歪了
3/暴光不足,樹脂偏軟,拉升變形 -
测量這排柱子的直徑可参考樹脂精度
如發現尺寸偏小, 可加层暴光
如發現尺寸偏大, 可减层暴光 -
假如垂直面孔不圆, 那就要调整抬升速度.
-
情况1: 機器Z絲杆步進值不准,或平台不平
情况2: 升速過快/暴光不足,导致孔拉变形 -
小字如果没有出現,那就是暴光不足
-
測膜粘力
-
打實際模型的参數最好是這兩個孔堵塞了
-
這排專測堆料,但假如清洗不到位,也會粘牢
-
這有一排細節小坑專測樹脂精度